Apply to PVC, polyurea, silicon PU
Construction method traditional spraying, rolling coating Mixing ratio, weight ratio A: B=15:1 (Construction after 5 minutes of mixing)
|
Item Number |
SQM-A01B02 |
|
surface gloss |
semi-light |
|
Component |
two |
|
Suggested thickness of the dry film layer |
150-200 µ m |
|
Water resistance |
No change in 30 days |
|
The substrate temperature(℃) |
15-25 |
|
Surface drying time(H) |
2 |
|
Real dry(H) |